Clean the area thoroughly.  Make sure the area is
dry before proceeding.
Striking docks, other  boats, or submerged ob-
jects could create a very hazardous situation or
severely damage the fiberglass. In the event an
object is struck below or near the waterline, pro-
ceed directly and cautiously to the nearest ser-
vice facility and remove the boat from the water.
Closely inspect the hull for damage. If the outer
fiberglass laminate was penetrated, repairs must
be made prior to relaunch.
NOTICE
Be sure the structure and the ambient tempera-
ture are above 60  degrees F (15 degrees C)
and the relative humidity below 70%  immedi-
ately before, during, and after the repair.
5.
6.
If the nick or gouge is deep and penetrates through
the gel coat,  fill the area with  fiberglass patching
paste.  Follow the directions on the can when mix-
ing the paste with the catalyst.
Occasionally, blisters, crazing, scratches, or damage to
the fiberglass can occur.  Repairs may be necessary to
correct the problem.
After the  gouge is filled  and has dried,  sand the
patched area.  Begin by using medium-fine grade
sandpaper. Progressively use finer grade sandpa-
per until the surface is very smooth.  If necessary,
add filler and then sand the surface again.
A.   Scratches
Scratches occur during normal use.  Below is a step by
step procedure to repair scratches.
7.
Apply two or three light coats of matching fiberglass
gel coat  to the  repaired area.   Enough  gel coat
should be used so that the entire area is covered.
1
.
Clean area with soap and water.
Apply a fine rubbing compound and buff.
.   Wax.
2.
The gel coat must be catalyzed using up to 2% MEK
Peroxide which can be purchased at a supplier han-
dling fiberglass reinforced products.  Contact your
Four Winns dealer for assistance.
3
If this does not work, clean the area and sand lightly with
to 600 wet or dry sandpaper and follow with rubbing
400
compound and wax.
8.
9.
After ample drying time, sand the area using very
fine wet/dry sandpaper.   If the appearance of the
area is still not satisfactory, repeat steps 2 through
B.   Gouges & Cracks
4
as necessary.
Stress cracks and crazing are the appearance of hairline
cracks in the gel coat surface. When present, these prob-
lems usually occur in the gel coat finish or the outer “skin
coat” fiberglass  laminate.   The  appearance of  these
cracks does not pose a threat to the structural integrity of
the boat.  In most cases, they are cosmetic and can be
treated.
If above the waterline, polish the area using a fiber-
glass rubbing compound and then wax.  If the re-
paired area is below the waterline, the area should
be primed and painted in accordance with the anti-
fouling paint manufacturer’s instructions.
Gel coat,  like paint, will  change colors with  time and
exposure  to sunlight  (ultraviolet).   For  this  reason,
“matching” gel coat obtained from Four Winns may not
Cosmetic surface damage can be repaired as follows:
1
.
Sand the surrounding area with medium or fine grit     match the gel color of a  boat that has been exposed.
sandpaper. Clean all marine growth, dirt, antifouling    However, this is the closest match commercially avail-
paint, etc. from  the immediate area.  DO  NOT ex-     able. Afiberglass  technician can tint the gel to be used
cessively scratch or gouge the surrounding area.
in the repair to provide a closer color match.
2.
Use a hard, pointed tool to open the gel crack. Take   More severe fiberglass damage, especially when struc-
care not to damage the surrounding gel coat.
tural, requires the expertise of an experienced fiberglass
repair technician.  See your Four Winns dealer for as-
sistance.
3.
Sand the crack or gouge so the edges are smooth
and will allow proper “feathering” of the area.
378 Vista™ Owner’s Manual
Section P
Page 4
Product Specification
CategoriesFour Winns Manuals, Four Winns Vista Manuals, Outboard Marine Corporation Manuals
Tags
Model Year2002, 2003, 2004, 2005, 2006, 2007, 2008
Download File
Please Enter the Security Characters Shown Below. Letters are Case Sensitive. Your download link will appear upon completing this step.
- 197 pages
Document TypeOwner's Manual
LanguageEnglish
Product BrandBoats and Cruisers, Four Winns. For support contact your dealer at http://www.fourwinns.com/locate-dealer.aspx
Document File TypePDF
Publisherfourwinns.com
Wikipedia's PageOutboard Marine Corporation
CopyrightAttribution Non-commercial
(1 votes, average: 4 out of 4)
Marine readers have rated 2002-2008 Four Winns Vista 378 Boat Owners Manual 4.0 out of 4.0 based on 1 product reviews.
Submit your review (optional)
(will not be displayed)
* Required Field

2002-2008 Four Winns Vista 378 Boat Owners Manual SKU UPC Model
shaun on Jul 07, 2014. s

great very informative. should not have to fill this out for a manule though


Leave a Reply

Your email address will not be published. Required fields are marked *

*
*
Website