Follow the instructions below for boats that have weath- To remove stains, refer to the procedures below.
ered and chalked.
1.
Wash area with hand dishwashing soap.
1.
2.
Wash.
2.
Begin with a small area such as three feet by three
feet and apply a mild cleanser.
Wax. If this does not work, then use a fine rubbing
compound. If this does not work use 400 or 600 wet
ordrysandpaper,followedbyfinerubbingcompound
and wax.
3.
4.
Rinse with clean water.
Follow with compound and waxing as outlined in
procedure above.
When using wax or fine rubbing compounds, make sure
to read the label and follow the directions. Some helpful
tips are listed below.
If the stain is not removed by the hand dishwashing soap
or mild cleanser, then the next procedure is to use either
1.
2.
Avoid working in direct sunlight. This dries out the denatured or rubbing alcohol. If this does not work, con-
wax or compound, and can stain the surface.
sult your Four Winns dealer for professional assistance.
Use clean pads or cloths to apply a thin coating of
wax or rubbing compound to a small area such as
three feet by three feet. Remove any excess, and
then rub the area with a buffing pad, or power buffer.
Apply pressure only as necessary to restore the
surface finish. Applying too much pressure or buff-
NOTICE
DO NOT use acetone, ketone, or other solvents
to remove stains. These chemicals are flam-
mable and may damage the gel coat.
ing in one place too long can permanently damage M - 5 FIBERGLASS REPAIRS
the surface.
Fiberglass is one of the most durable, strong, and for-
After applying compound, always follow with wax- giving construction materials afloat. It is resilient and
3.
ing.
normalrepairscanbemadewithoutaffectingthestrength
or structural integrity of the boat.
NOTICE
If using a power buffer, use a low RPM buffer
with light pressure. Keep the pad wet and the
buffer moving at all times to prevent heat build
up.
Striking docks, other boats, or submerged ob-
jects could create a very hazardous situation or
severely damage the fiberglass. In the event
an object is struck below or near the waterline,
proceed directly and cautiously to the nearest
service facility and remove the boat from the
water. Closely inspect the hull for damage. If
the outer fiberglass laminate was penetrated,
repairs must be made prior to re-launch.
NOTICE
When sanding, DO NOT use a power or belt
sander to prevent gouges, uneven areas, or
other damage. For best results, block sand the
gel coat.
C. Stains
Occasionally, blisters, crazing, scratches, or damage to
the fiberglass can occur. Repairs may be necessary to
correct the problem.
Stains can appear anywhere on the exterior of the boat
and may be a result of contact with tar, plant sap, leaves,
rust from metal fittings, and other materials. Surface
stains may be removed with hand dishwashing soap,
mild cleansers, or some household detergents. DO NOT
use chlorine or ammonia products. These products can
affect the color of gel coat. Commercial car washes use
strong cleaners and should be avoided.
A. Scratches
Scratches occur during normal use. Below is a step by
step procedure to repair scratches.
1.
Clean area with soap and water.
Vista Owners Manual
10/93
Section M
Page 3
Categories | Four Winns Manuals, Four Winns Vista Manuals, Outboard Marine Corporation Manuals |
---|---|
Tags | Four Winns Vista 238, Four Winns Vista 258, Four Winns Vista 278 |
Model Year | 2000 |
Download File |
|
Document Type | Owner's Manual |
Language | English |
Product Brand | Boats and Cruisers, Four Winns. For support contact your dealer at http://www.fourwinns.com/locate-dealer.aspx |
Document File Type | |
Publisher | fourwinns.com |
Wikipedia's Page | Outboard Marine Corporation |
Copyright | Attribution Non-commercial |
(0 votes, average: 0 out of 5)